{"efta_number": "EFTA01099281", "page_count": 2, "url": "https://epstein-data.com/EFTA01099281", "pdf_url": "https://epstein-data.com/pdf/EFTA01099281.pdf", "pages": [{"efta_number": "EFTA01099281", "page_number": 0, "text_content": "I.\nDETERMINING COVERAGE\nA.\nB.\nC.\nMeasure the total square footage of the pool's interior surface (walls and floor). Include\nextra material for steps, benches and swim outs.\nDetermine the required number of bags by using 25 square feet per bag for the average\npool. More material will be required for a rougher shell. Use 18 square feet per bag for\nPearl, Golden Pearl and Tahoe Blue Golden Pearl due to the larger aggregate size.\nAlways add 5% to 10% more bags to allow for error. It will not\nbe possible to match areas plastered later due to shortages on the\njob site. Always take more than you need.\nPREPARATION OF THE SUBSTRATE OR POOL SHELL\nII.\nA.\nNew Pool Shells\n1.\n2.\n3.\n5.\n6.\nThe shell must be free of any foreign material that may interfere with the bonding of the\nnew plaster.\nAll loose material such as dripped thinset, grout, paint, dirt, patching or decking products\nmust be removed by scraping, water blasting (pressure cleaning) or sand blasting.\nAlgae, mold and mildew must be eliminated by chlorine washing. Failure to do so will\nresult in discoloration and bond failure (delaminations).\nRemove any oil or grease with tri-sodium phosphate and water. Oils and grease left on\nthe pool shell will cause bond failure and prevent proper etching and cleaning by\nwaterborne acid solutions. To test for oil and grease, wet the entire pool shell surface and\nexamine it carefully for beading water droplets. Heavily saturated areas may require\nsoaking with liquid detergents until oil is removed.\nEtch the surface with Muriatic Acid and water. Adjust the concentration as needed to\nproperly clean and roughen the surface. Smoother shells will require a higher\nconcentration of acid and vice versa.\nAll water penetration due to hydrostatic pressure (weepers) must be stopped. Use SGM\nInstant Hydraulic Cement to plug leaks and seal around fittings.\n7.\nThe shell must be fully cured at least 28 days.\n8.\n9.\nAll pool inlets and main drain lines should be plugged to prevent clogging during\nplasterwork and exposure. All plugs except the main drain should remain in place until\nthe pool is filled to prevent drip stains.\nMark the location of all fittings with a small piece of tape placed on the coping directly\nabove to prevent them from being accidentally covered during the plaster process. It may\nbe best to draw a map indicating the locations of all fittings in projects with numerous\ninlets and outlets.\nB.\nResurfacing Projects\n1.\nFollow all of the above procedures.\n2.\nUndercut all existing tile and fittings 2\" away and 3/8\" deep into the existing plaster\nsubstrate.\n3\nEFTA01099281\n", "char_count": 2592}, {"efta_number": "EFTA01099281", "page_number": 1, "text_content": "3.\n4.\n5.\nIII.\nSound out and remove all hollow and delaminated plaster. Identify the hollow spots and\nsaw an area 3\" outside them. Remove the loose plaster inside the cut area.\nFill the hollow with SGM Vinyl Patching Compound or SGM Sand Topping Mix and\nConcrete Bonding Agent bringing the area level with the existing plaster.\nApply SGM Bond Kote as directed. Each unit of Bond Kote consists of one 5-gallon pail\nof Liquid Resin and two 65 lb., bags of Dry Mix and will cover approximately 500 square\nfeet. Mix one 65 lb. bag of SGM Bond Kote with 1/2 pail of SGM Bond Kote Liquid Resin.\nCoat existing plaster using a 1 1/4\" nap paint roller.\nAllow material to set for one minute then create stipple texture by going over the area\nagain with roller. Allow Bond Kote to cure for at least 6 hours before plastering. If Bond\nKote is rained on or left to sit for more than a few days it may have to be reapplied.\nMIXING\nNote: Diamond Brite is made in batches of 60 to 80 bags using natural ingredients. For this\nreason there will be variations in shade between batches. Batch numbers are stamped\non the ends of every bag. It is therefore incumbent upon the user to follow these\ninstructions explicitly to ensure the most consistent color throughout the pool.\nA.\nB.\nC.\nSeparate the bags according to the batch numbers stamped on the bottom of each bag.\nRecord all batch numbers. All warranties are rendered invalid without the batch\nnumbers.\nBlend different batches together in each mix according to the ratio present at the job site.\nFor example: If there are 30 bags total on the job and there are 20 bags of Batch A and\n10 bags of Batch B then use 2 bags of A to 1 bag of B in every mix.\nMeasure and add water to mixer. Hold back a portion of the water and add as necessary\nas mixing progresses. Careful measuring of the mix water will produce the best material.\nLower water to cement ratios will produce plaster of greater strength and density. It is\ntherefore best to use as little water as needed to produce a workable mix. Excess water\nwill reduce strength and increase shrinkage (check) cracks. Water requirements will vary\naccording to job site conditions.\nXX - Note: Mix water quality is extremely important. Well water or water high in metal and mineral\nD.\nE.\nF.\ncontent will cause discoloration in finished Diamond Brite. Additionally, mix water of high\nhardness or alkalinity will cause the plaster to effloresce, releasing high levels of salts that\nproduce calcium scale. This is especially true of colored Diamond Brite such as Midnite\nBlue, Onyx, Tahoe Blue and French Gray. Check mix water for metals, minerals,\nhardness and alkalinity before using.\nStart mixer and add Diamond Brite as quickly as possibly to ensure that all the material\nhas the proper mix time. Failure to do so will produce uneven set times and result in\nwashouts and streaking.\nMix for a minimum of 5 minutes but no more than 10 minutes. This ensures even\ndistribution of aggregates and increases the working time of the plaster. Insufficient mix\ntime will result in uneven setting and shade variations. Too much mix time will produce\nan overall weaker plaster and may entrain undesirable air bubbles. As a rule of thumb,\nmix for only the amount of time required to produce a consistent, homogenous batter.\nCalcium Chloride may be used as an accelerator. It must be fully dissolved in water\nallowing impurities to settle out. Pour off the solution from the top being careful not to add\nimpurities to the mix. The impurities found in calcium chloride flake and pellets have\nEFTA01099282\n", "char_count": 3569}]}